China 6013 Ac Welding Rod 1/8 3/32 5/32
Applications
Suitable for welding of low carbon steel structure,especially for the welding of thin plate steel with short discontinuous weld and requirement of smooth welding pass.
Notes on usage
1.Generally, welding rods do not need to be baked before welding.
2.After being exposed to moisture, bake at 150℃-170℃ for 0.5-1 hour before use
Description
Model | GB | AWS | Diameter(mm) | Type of Coating | Current |
CB-J421 | E4313 | E6013 | 1/8 3/32 5/32 | Titania Type | AC DC |
Chemical Composition of Deposited Metal (%)
C | Mn | Si | S | P |
≤0.12 | 0.3-0.6 | ≤0.35 | ≤0.035 | ≤0.040 |
Mechanical Properties of Deposited Metal
Tensile Strength(Mpa) | Elongation(%) |
460-540 | 18-26 |
Packing
Our Factory
Exhibition
Our Certification