China Eletrodo 6013
Applications
Suitable for low carbon steel structure,especially for the welding of thin plate steel with short discontinuous weld and requirement of smooth welding pass.
Notes on usage
1.Generally, welding rods do not need to be baked before welding.
2.After being exposed to moisture, bake at 150℃-170℃ for 0.5-1 hour before use
Description
Model | GB | AWS | Diameter(mm) | Type of Coating | Current | Uses |
CB-J421 | E4313 | E6013 | 2.5-5.0 | Rutile type | AC/DC | Suitable for low carbon steel structure,especially for the welding of thin plate steel with short discontinuous weld and requirement of smooth welding pass. |
Chemical Composition of Deposited Metal (%)
C | Mn | Si | S | P | Cr | Ni | Mo |
0.08 | 0.37 | 0.18 | 0.020 | 0.025 | 0.035 | 0.030 | 0.005 |
Mechanical Properties of Deposited Metal
Tensile Strength(Mpa) | Elongation(%) |
500 | 27 |