Copper Bridge Brand Welding Rod 3/32 7018

J508(J506Fe)
● Iron powder low hydrogen potassium type
● Easy to ignite an arc
● Must be baked at 350℃ for 1 hour before welding

  • FOB Price: US $0.5 - 9,999 / Piece
  • Min.Order Quantity: 100 Piece/Pieces
  • Supply Ability: 10000 Piece/Pieces per Month
  • Product Detail

    Product Tags

    Applications

    Suitable for welding important carbon steel and low alloy steel

    Notes on usage

    1. Before welding, the welding rod must be baked at 350℃ for 1 hour and used immediately after baking.
    2. Before welding, the weldment must be cleaned of rust, oil, moisture and other impurities.
    3. Use short arc operation and narrow channel welding.

    Description

    Model GB AWS Diameter(mm) Type of Coating Current
    CB-J508 E5018 E7018 1/8 3/32 5/32 Low-hydrogen Type AC DC

    Chemical Composition of Deposited Metal (%)

    C Mn Si S P Cr Ni Mo
    ---- ≤1.60 ≤0.75 ≤0.035 ≤0.040 ≤0.20 ≤0.30 ≤0.30
    0.065 1.38 0.44 0.012 0.020 0.011 0.015 0.001

    Mechanical Properties of Deposited Metal

    Tensile Strength(Mpa) Elongation(%)
    460 31

    Packing

    packing (1)

    微信图片_20240718152717

    Our Factory

    4e0eaf6c11aec2283e8aa8c3240e8d0

    微信图片_20240718124759

    Exhibition

    82752267979566337

    c6c33ad21dea9139e01ecb29575a8e7

    ae (1)

    9a

    9a

    9a

    9a

    9a

    Our Certification

    2

    1

    3

    4






  • Previous:
  • Next:

  • Write your message here and send it to us