Copper Bridge Brand Welding Rod Aws 6011
Applications
Suitable for butt, fillet and lap welding of thin plate structures
Notes on usage
1.Generally, welding rods do not need to be baked before welding.
2.After being exposed to moisture, bake at 70-80℃ for 0.5-1 hour before use
Description
Model | GB | AWS | Diameter(mm) | Type of Coating | Current |
CB-J425 | E4311 | E6011 | 2.5-5.0 | High cellulose potassium type | AC/DC |
Chemical Composition of Deposited Metal (%)
C | Mn | Si | S | P |
0.09 | 0.065 | 0.20 | 0.023 | 0.025 |
Mechanical Properties of Deposited Metal
Tensile Strength(Mpa) | Elongation(%) |
415 | 26 |
Packing